Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico Rp0.5 | 20.0 °C | 125 - 140 MPa Show Material materials with Límite elástico Rp0.5 of 125 - 140 MPa |
Resistencia a la tracción | 20.0 °C | 345 MPa Show Material materials with Resistencia a la tracción of 345 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 125 - 140 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 125 - 140 MPa |