Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 30 - 35 % Show Material materials with Elongación A50 of 30 - 35 % |
Límite elástico Rp0.5 | 20.0 °C | 195 - 255 MPa Show Material materials with Límite elástico Rp0.5 of 195 - 255 MPa |
Resistencia a la tracción | 20.0 °C | 450 - 515 MPa Show Material materials with Resistencia a la tracción of 450 - 515 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 180 - 250 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 180 - 250 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 6 - 7.5 % Show Material materials with Aluminio of 6 - 7.5 % |
Estaño | 0.2 - 0.5 % Show Material materials with Estaño of 0.2 - 0.5 % |
Hierro | 2 - 3 % Show Material materials with Hierro of 2 - 3 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 0.15 % Show Material materials with Níquel of 0.15 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |