Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico Rp0.5 | 20.0 °C | 195 - 205 MPa Show Material materials with Límite elástico Rp0.5 of 195 - 205 MPa |
Resistencia a la tracción | 20.0 °C | 450 - 485 MPa Show Material materials with Resistencia a la tracción of 450 - 485 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 180 - 195 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 180 - 195 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 6 - 8 % Show Material materials with Aluminio of 6 - 8 % |
Hierro | 1.5 - 3.5 % Show Material materials with Hierro of 1.5 - 3.5 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |