Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 10 % Show Material materials with Elongación A50 of 10 % |
Límite elástico Rp0.5 | 20.0 °C | 205 - 250 MPa Show Material materials with Límite elástico Rp0.5 of 205 - 250 MPa |
Resistencia a la tracción | 20.0 °C | 550 - 620 MPa Show Material materials with Resistencia a la tracción of 550 - 620 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 195 - 235 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 195 - 235 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 8.7 - 9.5 % Show Material materials with Aluminio of 8.7 - 9.5 % |
Hierro | 3.5 - 4.3 % Show Material materials with Hierro of 3.5 - 4.3 % |
Manganeso | 1.2 - 2 % Show Material materials with Manganeso of 1.2 - 2 % |
Níquel | 4 - 4.8 % Show Material materials with Níquel of 4 - 4.8 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |