Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 30 % Show Material materials with Elongación A50 of 30 % |
Límite elástico Rp0.5 | 20.0 °C | 125 - 140 MPa Show Material materials with Límite elástico Rp0.5 of 125 - 140 MPa |
Resistencia a la tracción | 20.0 °C | 310 - 345 MPa Show Material materials with Resistencia a la tracción of 310 - 345 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 125 - 140 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 125 - 140 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 65 % Show Material materials with Cobre of 65 % |
Hierro | 0.4 - 1 % Show Material materials with Hierro of 0.4 - 1 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 29 - 33 % Show Material materials with Níquel of 29 - 33 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |