Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico Rp0.5 | 20.0 °C | 110 MPa Show Material materials with Límite elástico Rp0.5 of 110 MPa |
Resistencia a la tracción | 20.0 °C | 290 MPa Show Material materials with Resistencia a la tracción of 290 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 110 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 110 MPa |
Chemical properties
Property | Value |
---|---|
Cromo | 0.3 - 0.7 % Show Material materials with Cromo of 0.3 - 0.7 % |
Hierro | 0.5 - 1 % Show Material materials with Hierro of 0.5 - 1 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Níquel | 15 - 18 % Show Material materials with Níquel of 15 - 18 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |