General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Dureza Rockwell B | 23.0 °C | 85 - 90 [-] Show Material materials with Dureza Rockwell B of 85 - 90 [-] | |
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % | |
Energía de impacto Charpy | 23.0 °C | 95 J Show Material materials with Energía de impacto Charpy of 95 J | |
Límite elástico Rp 0,2 | 23.0 °C | 207 MPa Show Material materials with Límite elástico Rp 0,2 of 207 MPa | |
Módulo elástico | 23.0 °C | 108 GPa Show Material materials with Módulo elástico of 108 GPa | |
Resistencia a la tracción | 23.0 °C | 379 MPa Show Material materials with Resistencia a la tracción of 379 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 23.0 °C | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.15 % Show Material materials with Aluminio of 0.15 % |
Antimonio | 0.05 % Show Material materials with Antimonio of 0.05 % |
Arsénico | 0.05 % Show Material materials with Arsénico of 0.05 % |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Cobre | 80 % Show Material materials with Cobre of 80 % |
Estaño | 0.25 % Show Material materials with Estaño of 0.25 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Magnesio | 0.01 % Show Material materials with Magnesio of 0.01 % |
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % |
Níquel | 0.2 % Show Material materials with Níquel of 0.2 % |
Plomo | 0.09 % Show Material materials with Plomo of 0.09 % |
Silicona | 3.8 - 4.2 % Show Material materials with Silicona of 3.8 - 4.2 % |
Zinc | 12 - 16 % Show Material materials with Zinc of 12 - 16 % |