Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 24 [-] Show Material materials with Dureza Rockwell C of 24 [-] | |
Elongación A50 | 23.0 °C | 12 % Show Material materials with Elongación A50 of 12 % | |
Hardness, Rockwell Superficial 15-N | 23.0 °C | 72 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 72 [-] | |
Hardness, Rockwell Superficial 30-N | 23.0 °C | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 45 [-] | |
Límite elástico | 23.0 °C | 655 - 860 MPa Show Material materials with Límite elástico of 655 - 860 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 825 - 930 MPa Show Material materials with Resistencia a la tracción of 825 - 930 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % |
Berilio | 1.6 - 1.85 % Show Material materials with Berilio of 1.6 - 1.85 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |