Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell C | 23.0 °C | 33 [-] Show Material materials with Dureza Rockwell C of 33 [-] | |
Elongación A50 | 23.0 °C | 3 % Show Material materials with Elongación A50 of 3 % | |
Hardness, Rockwell Superficial 15-N | 23.0 °C | 76.5 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 76.5 [-] | |
Hardness, Rockwell Superficial 30-N | 23.0 °C | 53 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 53 [-] | |
Límite elástico | 23.0 °C | 1035 - 1240 MPa Show Material materials with Límite elástico of 1035 - 1240 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 1210 - 1310 MPa Show Material materials with Resistencia a la tracción of 1210 - 1310 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |