Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 200 [-] Show Material materials with Dureza Brinell of 200 [-] |
Elongación A50 | 20.0 °C | 5 % Show Material materials with Elongación A50 of 5 % |
Límite elástico Rp0.5 | 20.0 °C | 415 MPa Show Material materials with Límite elástico Rp0.5 of 415 MPa |
Resistencia a la tracción | 20.0 °C | 760 MPa Show Material materials with Resistencia a la tracción of 760 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 10 - 11.5 % Show Material materials with Aluminio of 10 - 11.5 % |
Cobre | 78 % Show Material materials with Cobre of 78 % |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % |
Manganeso | 3.5 % Show Material materials with Manganeso of 3.5 % |
Níquel | 3 - 5.5 % Show Material materials with Níquel of 3 - 5.5 % |