General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Densidad of 8.4 - 8.9 g/cm³ | Typical for Cast Copper Nickel Silver Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.32 [-] Show Material materials with Coeficiente de Poisson of 0.32 [-] | Typical for Cast Copper Nickel Silver Grade |
Elongación A50 | 23.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | |
Límite elástico Rp0.5 | 23.0 °C | 97 MPa Show Material materials with Límite elástico Rp0.5 of 97 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Nickel Silver Grade |
Resistencia a la tracción | 23.0 °C | 207 MPa Show Material materials with Resistencia a la tracción of 207 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Cast Copper Nickel Silver Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Nickel Silver Grade |
Conductividad térmica | 23.0 °C | 22 - 29 W/(m·K) Show Material materials with Conductividad térmica of 22 - 29 W/(m·K) | Typical for Cast Copper Nickel Silver Grade |
Temperatura de fusión | 1010 - 1180 °C Show Material materials with Temperatura de fusión of 1010 - 1180 °C | Typical for Cast Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.35 % Show Material materials with Antimonio of 0.35 % |
Azufre | 0.08 % Show Material materials with Azufre of 0.08 % |
Cobre | 53 - 58 % Show Material materials with Cobre of 53 - 58 % |
Estaño | 1.5 - 3 % Show Material materials with Estaño of 1.5 - 3 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 1.5 % Show Material materials with Hierro of 1.5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 11 - 14 % Show Material materials with Níquel of 11 - 14 % |
Plomo | 8 - 11 % Show Material materials with Plomo of 8 - 11 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Zinc | 17 - 25 % Show Material materials with Zinc of 17 - 25 % |