Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Hardness, Rockwell F | 20.0 °C | 40 [-] Show Material materials with Hardness, Rockwell F of 40 [-] |
Límite elástico Rp0.5 | 20.0 °C | 85 MPa Show Material materials with Límite elástico Rp0.5 of 85 MPa |
Resistencia a la tracción | 20.0 °C | 235 MPa Show Material materials with Resistencia a la tracción of 235 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 99.9 % Show Material materials with Cobre of 99.9 % |
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Telurio | 0.4 - 0.7 % Show Material materials with Telurio of 0.4 - 0.7 % |