Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Hardness, Rockwell F | 20.0 °C | 40 [-] Show Material materials with Hardness, Rockwell F of 40 [-] |
Límite elástico Rp0.5 | 20.0 °C | 85 MPa Show Material materials with Límite elástico Rp0.5 of 85 MPa |
Resistencia a la tracción | 20.0 °C | 235 MPa Show Material materials with Resistencia a la tracción of 235 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.2 - 0.5 % Show Material materials with Azufre of 0.2 - 0.5 % |
Cobre | 99.9 % Show Material materials with Cobre of 99.9 % |
Fósforo | 2E-3 - 5E-3 % Show Material materials with Fósforo of 2E-3 - 5E-3 % |