Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 45 [-] Show Material materials with Dureza Rockwell B of 45 [-] |
Elongación A50 | 20.0 °C | 40 % Show Material materials with Elongación A50 of 40 % |
Límite elástico Rp0.5 | 20.0 °C | 160 MPa Show Material materials with Límite elástico Rp0.5 of 160 MPa |
Resistencia a la tracción | 20.0 °C | 400 MPa Show Material materials with Resistencia a la tracción of 400 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 58 - 61 % Show Material materials with Cobre of 58 - 61 % |
Estaño | 0.25 % Show Material materials with Estaño of 0.25 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Plomo | 0.25 - 0.7 % Show Material materials with Plomo of 0.25 - 0.7 % |