Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 82 [-] Show Material materials with Dureza Rockwell B of 82 [-] |
Elongación A50 | 20.0 °C | 32 % Show Material materials with Elongación A50 of 32 % |
Límite elástico Rp0.5 | 20.0 °C | 255 MPa Show Material materials with Límite elástico Rp0.5 of 255 MPa |
Resistencia a la tracción | 20.0 °C | 565 MPa Show Material materials with Resistencia a la tracción of 565 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 8.5 - 10 % Show Material materials with Aluminio of 8.5 - 10 % |
Estaño | 0.6 % Show Material materials with Estaño of 0.6 % |
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |