Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 77 [-] Show Material materials with Dureza Rockwell B of 77 [-] |
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico Rp0.5 | 20.0 °C | 285 MPa Show Material materials with Límite elástico Rp0.5 of 285 MPa |
Resistencia a la tracción | 20.0 °C | 570 MPa Show Material materials with Resistencia a la tracción of 570 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 6.3 - 7 % Show Material materials with Aluminio of 6.3 - 7 % |
Arsénico | 0.09 % Show Material materials with Arsénico of 0.09 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 1.5 - 2 % Show Material materials with Silicona of 1.5 - 2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |