Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell B | 20.0 °C | 69 [-] Show Material materials with Dureza Rockwell B of 69 [-] |
Elongación A50 | 20.0 °C | 33 % Show Material materials with Elongación A50 of 33 % |
Límite elástico Rp0.5 | 20.0 °C | 235 MPa Show Material materials with Límite elástico Rp0.5 of 235 MPa |
Resistencia a la tracción | 20.0 °C | 495 MPa Show Material materials with Resistencia a la tracción of 495 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 57 - 60 % Show Material materials with Cobre of 57 - 60 % |
Estaño | 0.5 - 1.5 % Show Material materials with Estaño of 0.5 - 1.5 % |
Hierro | 0.4 - 1.3 % Show Material materials with Hierro of 0.4 - 1.3 % |
Manganeso | 0.05 - 0.5 % Show Material materials with Manganeso of 0.05 - 0.5 % |
Plomo | 0.5 - 1 % Show Material materials with Plomo of 0.5 - 1 % |