General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Elongación A50 | 23.0 °C | 4 - 12 % Show Material materials with Elongación A50 of 4 - 12 % | |
Límite elástico Rp0.5 | 23.0 °C | 105 - 275 MPa Show Material materials with Límite elástico Rp0.5 of 105 - 275 MPa | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 95 - 98 GPa Show Material materials with Módulo elástico of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Resistencia a la tracción | 23.0 °C | 220 - 330 MPa Show Material materials with Resistencia a la tracción of 220 - 330 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
Property | Value |
---|---|
Cobre | 99.85 % Show Material materials with Cobre of 99.85 % |
Fósforo | 0.01 - 0.03 % Show Material materials with Fósforo of 0.01 - 0.03 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Telurio | 0.3 - 0.7 % Show Material materials with Telurio of 0.3 - 0.7 % |