Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 20 % Show Material materials with Elongación A50 of 20 % |
Límite elástico Rp0.5 | 20.0 °C | 170 MPa Show Material materials with Límite elástico Rp0.5 of 170 MPa |
Resistencia a la tracción | 20.0 °C | 310 MPa Show Material materials with Resistencia a la tracción of 310 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 1 - 1.8 % Show Material materials with Hierro of 1 - 1.8 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Niobio | 1 % Show Material materials with Niobio of 1 % |
Níquel | 9 - 11 % Show Material materials with Níquel of 9 - 11 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |