General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Elongación A50 | 23.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | |
Límite elástico Rp0.5 | 23.0 °C | 485 - 515 MPa Show Material materials with Límite elástico Rp0.5 of 485 - 515 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 23.0 °C | 550 - 620 MPa Show Material materials with Resistencia a la tracción of 550 - 620 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 1.6 - 2.2 % Show Material materials with Níquel of 1.6 - 2.2 % |
Plomo | 0.09 % Show Material materials with Plomo of 0.09 % |
Silicona | 0.4 - 0.8 % Show Material materials with Silicona of 0.4 - 0.8 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |