Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 49 - 70 [-] Show Material materials with Dureza Rockwell B of 49 - 70 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 51 - 66 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 51 - 66 [-] | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 365 - 435 MPa Show Material materials with Resistencia a la tracción of 365 - 435 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Cobre | 97 % Show Material materials with Cobre of 97 % |
Fósforo | 0.02 - 0.15 % Show Material materials with Fósforo of 0.02 - 0.15 % |
Hierro | 2.1 - 2.6 % Show Material materials with Hierro of 2.1 - 2.6 % |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % |
Zinc | 0.05 - 0.2 % Show Material materials with Zinc of 0.05 - 0.2 % |