Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 84 - 87 [-] Show Material materials with Dureza Rockwell B of 84 - 87 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 74 - 77 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 74 - 77 [-] | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 605 - 670 MPa Show Material materials with Resistencia a la tracción of 605 - 670 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Cobalto | 0.3 - 1.3 % Show Material materials with Cobalto of 0.3 - 1.3 % |
Cobre | 96 % Show Material materials with Cobre of 96 % |
Estaño | 0.1 - 1 % Show Material materials with Estaño of 0.1 - 1 % |
Fósforo | 0.01 - 0.35 % Show Material materials with Fósforo of 0.01 - 0.35 % |
Hierro | 1 - 2 % Show Material materials with Hierro of 1 - 2 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |