Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 66 - 73 [-] Show Material materials with Dureza Rockwell B of 66 - 73 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 65 - 70 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 65 - 70 [-] | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 415 - 485 MPa Show Material materials with Resistencia a la tracción of 415 - 485 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Cobalto | 0.05 % Show Material materials with Cobalto of 0.05 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Fósforo | 0.1 - 0.4 % Show Material materials with Fósforo of 0.1 - 0.4 % |
Hierro | 0.3 - 1.2 % Show Material materials with Hierro of 0.3 - 1.2 % |
Magnesio | 0.01 - 0.2 % Show Material materials with Magnesio of 0.01 - 0.2 % |
Manganeso | 0.05 % Show Material materials with Manganeso of 0.05 % |
Níquel | 0.05 % Show Material materials with Níquel of 0.05 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |