General
Property | Value | Comment |
---|---|---|
Densidad | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Tamaño de grano | 0.0307 μm Show Material materials with Tamaño de grano of 0.0307 μm | Predicted Value |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass | ||
Dureza Brinell | 162 [-] Show Material materials with Dureza Brinell of 162 [-] | Predicted Value | ||
Dureza Brinell (HBW) | 237.8 [-] Show Material materials with Dureza Brinell (HBW) of 237.8 [-] | Predicted Value | ||
Dureza Vickers | 141 [-] Show Material materials with Dureza Vickers of 141 [-] | Predicted Value | ||
Estricción | 35.8 % Show Material materials with Estricción of 35.8 % | Predicted Value | ||
Hardness, Rockwell F | 78 [-] Show Material materials with Hardness, Rockwell F of 78 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 70 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 70 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 42 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 42 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 78 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 78 [-] | Predicted Value | ||
Módulo de cizallamiento | 43.7 GPa Show Material materials with Módulo de cizallamiento of 43.7 GPa | Predicted Value | ||
Módulo elástico | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass | ||
Resistencia a la compresión | 1151 MPa Show Material materials with Resistencia a la compresión of 1151 MPa | Predicted Value | ||
Resistencia a la fatiga | 378 MPa Show Material materials with Resistencia a la fatiga of 378 MPa | Predicted Value | ||
Resistencia a la tracción | 621 MPa Show Material materials with Resistencia a la tracción of 621 MPa | ASTM B505 | Casting | |
Resistencia al cizallamiento | 366 MPa Show Material materials with Resistencia al cizallamiento of 366 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 1.5e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5e-05 - 1.9e-05 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Eléctrico
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 3 - 4.9 % Show Material materials with Aluminio of 3 - 4.9 % | ASTM B505 | Casting |
Cobre | 60 - 66 % Show Material materials with Cobre of 60 - 66 % | ASTM B505 | Casting |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % | ASTM B505 | Casting |
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % | ASTM B505 | Casting |
Manganeso | 2.5 - 5 % Show Material materials with Manganeso of 2.5 - 5 % | ASTM B505 | Casting |
Níquel | 1 % Show Material materials with Níquel of 1 % | ASTM B505 | Casting |
Plomo | 0.2 % Show Material materials with Plomo of 0.2 % | ASTM B505 | Casting |
Zinc | 22 - 28 % Show Material materials with Zinc of 22 - 28 % | ASTM B505 | Casting |