General
Property | Value | Comment |
---|---|---|
Densidad | 8.62 g/cm³ Show Material materials with Densidad of 8.62 g/cm³ | Predicted Value |
Tamaño de grano | 0.031 μm Show Material materials with Tamaño de grano of 0.031 μm | Predicted Value |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze | ||
Dureza Brinell | 110 [-] Show Material materials with Dureza Brinell of 110 [-] | Predicted Value | ||
Dureza Brinell (HBW) | 249.8 [-] Show Material materials with Dureza Brinell (HBW) of 249.8 [-] | Predicted Value | ||
Dureza Vickers | 129 [-] Show Material materials with Dureza Vickers of 129 [-] | Predicted Value | ||
Estricción | 58.4 % Show Material materials with Estricción of 58.4 % | Predicted Value | ||
Hardness, Rockwell F | 80 [-] Show Material materials with Hardness, Rockwell F of 80 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 45 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 55 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 55 [-] | Predicted Value | ||
Módulo de cizallamiento | 45.0 GPa Show Material materials with Módulo de cizallamiento of 45.0 GPa | Predicted Value | ||
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Resistencia a la compresión | 1215 MPa Show Material materials with Resistencia a la compresión of 1215 MPa | Predicted Value | ||
Resistencia a la fatiga | 395 MPa Show Material materials with Resistencia a la fatiga of 395 MPa | Predicted Value | ||
Resistencia a la tracción | 276 MPa Show Material materials with Resistencia a la tracción of 276 MPa | ASTM B505 | Casting | |
Resistencia al cizallamiento | 236.7 MPa Show Material materials with Resistencia al cizallamiento of 236.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Eléctrico
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.005 % Show Material materials with Aluminio of 0.005 % | ASTM B505 | Casting |
Antimonio | 0.2 % Show Material materials with Antimonio of 0.2 % | ASTM B505 | Casting |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % | ASTM B505 | Casting |
Cobre | 88 - 90 % Show Material materials with Cobre of 88 - 90 % | ASTM B505 | Casting |
Estaño | 10 - 12 % Show Material materials with Estaño of 10 - 12 % | ASTM B505 | Casting |
Fósforo | 1.5 % Show Material materials with Fósforo of 1.5 % | ASTM B505 | Casting |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % | ASTM B505 | Casting |
Níquel | 0.5 % Show Material materials with Níquel of 0.5 % | ASTM B505 | Casting |
Plomo | 0.5 % Show Material materials with Plomo of 0.5 % | ASTM B505 | Casting |
Silicona | 0.005 % Show Material materials with Silicona of 0.005 % | ASTM B505 | Casting |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % | ASTM B505 | Casting |