Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze |
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Límite elástico Rp0.5 | 23.0 °C | 165 MPa Show Material materials with Límite elástico Rp0.5 of 165 MPa | |
Módulo elástico | 23.0 °C | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze |
Resistencia a la tracción | 23.0 °C | 276 MPa Show Material materials with Resistencia a la tracción of 276 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.9E-5 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 23.0 °C | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.25 % Show Material materials with Antimonio of 0.25 % |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Cobre | 85 - 88 % Show Material materials with Cobre of 85 - 88 % |
Estaño | 10 - 12 % Show Material materials with Estaño of 10 - 12 % |
Fósforo | 1.5 % Show Material materials with Fósforo of 1.5 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Níquel | 0.8 - 1.5 % Show Material materials with Níquel of 0.8 - 1.5 % |
Plomo | 1 - 1.5 % Show Material materials with Plomo of 1 - 1.5 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |