General
Property | Value | Comment |
---|---|---|
Densidad | 8.622 g/cm³ Show Material materials with Densidad of 8.622 g/cm³ | Predicted Value |
Tamaño de grano | 0.0309 μm Show Material materials with Tamaño de grano of 0.0309 μm | Predicted Value |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze | ||
Dureza Brinell | 107 [-] Show Material materials with Dureza Brinell of 107 [-] | Predicted Value | ||
Dureza Brinell (HBW) | 249.7 [-] Show Material materials with Dureza Brinell (HBW) of 249.7 [-] | Predicted Value | ||
Dureza Vickers | 127 [-] Show Material materials with Dureza Vickers of 127 [-] | Predicted Value | ||
Estricción | 57.3 % Show Material materials with Estricción of 57.3 % | Predicted Value | ||
Hardness, Rockwell F | 77 [-] Show Material materials with Hardness, Rockwell F of 77 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 45 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 45 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 52 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 52 [-] | Predicted Value | ||
Módulo de cizallamiento | 46.0 GPa Show Material materials with Módulo de cizallamiento of 46.0 GPa | Predicted Value | ||
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Resistencia a la compresión | 1215 MPa Show Material materials with Resistencia a la compresión of 1215 MPa | Predicted Value | ||
Resistencia a la fatiga | 392 MPa Show Material materials with Resistencia a la fatiga of 392 MPa | Predicted Value | ||
Resistencia a la tracción | 252 MPa Show Material materials with Resistencia a la tracción of 252 MPa | ASTM B505 | Casting | |
Resistencia al cizallamiento | 224.1 MPa Show Material materials with Resistencia al cizallamiento of 224.1 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Eléctrico
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.005 % Show Material materials with Aluminio of 0.005 % | ASTM B505 | Casting |
Antimonio | 0.25 % Show Material materials with Antimonio of 0.25 % | ASTM B505 | Casting |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % | ASTM B505 | Casting |
Cobre | 86 - 89 % Show Material materials with Cobre of 86 - 89 % | ASTM B505 | Casting |
Estaño | 9 - 11 % Show Material materials with Estaño of 9 - 11 % | ASTM B505 | Casting |
Fósforo | 1.5 % Show Material materials with Fósforo of 1.5 % | ASTM B505 | Casting |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % | ASTM B505 | Casting |
Níquel | 1 % Show Material materials with Níquel of 1 % | ASTM B505 | Casting |
Plomo | 1 - 2.5 % Show Material materials with Plomo of 1 - 2.5 % | ASTM B505 | Casting |
Silicona | 0.005 % Show Material materials with Silicona of 0.005 % | ASTM B505 | Casting |