General
Property | Value | Comment |
---|---|---|
Densidad | 7.677 g/cm³ Show Material materials with Densidad of 7.677 g/cm³ | Predicted Value |
Tamaño de grano | 0.0293 μm Show Material materials with Tamaño de grano of 0.0293 μm | Predicted Value |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze | ||
Dureza Brinell | 141 [-] Show Material materials with Dureza Brinell of 141 [-] | Predicted Value | ||
Dureza Brinell (HBW) | 259.7 [-] Show Material materials with Dureza Brinell (HBW) of 259.7 [-] | Predicted Value | ||
Dureza Vickers | 143 [-] Show Material materials with Dureza Vickers of 143 [-] | Predicted Value | ||
Estricción | 47.0 % Show Material materials with Estricción of 47.0 % | Predicted Value | ||
Hardness, Rockwell F | 75 [-] Show Material materials with Hardness, Rockwell F of 75 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 70 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 70 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 43 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 43 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 67 [-] | Predicted Value | ||
Módulo de cizallamiento | 43.5 GPa Show Material materials with Módulo de cizallamiento of 43.5 GPa | Predicted Value | ||
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze | ||
Resistencia a la compresión | 1201 MPa Show Material materials with Resistencia a la compresión of 1201 MPa | Predicted Value | ||
Resistencia a la fatiga | 404 MPa Show Material materials with Resistencia a la fatiga of 404 MPa | Predicted Value | ||
Resistencia a la tracción | 469 MPa Show Material materials with Resistencia a la tracción of 469 MPa | ASTM B505 | Casting | |
Resistencia al cizallamiento | 317.8 MPa Show Material materials with Resistencia al cizallamiento of 317.8 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Eléctrico
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 8.5 - 9.5 % Show Material materials with Aluminio of 8.5 - 9.5 % | ASTM B505 | Casting |
Cobre | 86 % Show Material materials with Cobre of 86 % | ASTM B505 | Casting |
Hierro | 2.5 - 4 % Show Material materials with Hierro of 2.5 - 4 % | ASTM B505 | Casting |