General
Property | Value | Comment |
---|---|---|
Densidad | 7.631 g/cm³ Show Material materials with Densidad of 7.631 g/cm³ | Predicted Value |
Tamaño de grano | 0.031 μm Show Material materials with Tamaño de grano of 0.031 μm | Predicted Value |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze | |||
Dureza Brinell | 183 [-] Show Material materials with Dureza Brinell of 183 [-] | Predicted Value | |||
Dureza Brinell (HBW) | 237.8 [-] Show Material materials with Dureza Brinell (HBW) of 237.8 [-] | Predicted Value | |||
Dureza Vickers | 203 [-] Show Material materials with Dureza Vickers of 203 [-] | Predicted Value | |||
Estricción | 36.5 % Show Material materials with Estricción of 36.5 % | Predicted Value | |||
Hardness, Rockwell F | 79 [-] Show Material materials with Hardness, Rockwell F of 79 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 15-N | 73 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 73 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-N | 46 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 46 [-] | Predicted Value | |||
Hardness, Rockwell Superficial 30-T | 78 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 78 [-] | Predicted Value | |||
Módulo de cizallamiento | 46.2 GPa Show Material materials with Módulo de cizallamiento of 46.2 GPa | Predicted Value | |||
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze | |||
Resistencia a la compresión | 1184 MPa Show Material materials with Resistencia a la compresión of 1184 MPa | Predicted Value | |||
Resistencia a la fatiga | 380 MPa Show Material materials with Resistencia a la fatiga of 380 MPa | Predicted Value | |||
Resistencia a la tracción | 655 MPa Show Material materials with Resistencia a la tracción of 655 MPa | Heat-Treated | ASTM B505 | Casting | |
Resistencia al cizallamiento | 368.5 MPa Show Material materials with Resistencia al cizallamiento of 368.5 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminio | 10 - 11.5 % Show Material materials with Aluminio of 10 - 11.5 % | Heat-Treated | ASTM B505 | Casting |
Cobre | 78 % Show Material materials with Cobre of 78 % | Heat-Treated | ASTM B505 | Casting |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % | Heat-Treated | ASTM B505 | Casting |
Manganeso | 3.5 % Show Material materials with Manganeso of 3.5 % | Heat-Treated | ASTM B505 | Casting |
Níquel | 3 - 5.5 % Show Material materials with Níquel of 3 - 5.5 % | Heat-Treated | ASTM B505 | Casting |