General
Property | Value | Comment |
---|---|---|
Densidad | 7.592 g/cm³ Show Material materials with Densidad of 7.592 g/cm³ | Predicted Value |
Tamaño de grano | 0.0311 μm Show Material materials with Tamaño de grano of 0.0311 μm | Predicted Value |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Bronze |
Dureza Brinell | 155 [-] Show Material materials with Dureza Brinell of 155 [-] | Predicted Value |
Dureza Brinell (HBW) | 251.3 [-] Show Material materials with Dureza Brinell (HBW) of 251.3 [-] | Predicted Value |
Dureza Vickers | 236 [-] Show Material materials with Dureza Vickers of 236 [-] | Predicted Value |
Estricción | 35.7 % Show Material materials with Estricción of 35.7 % | Predicted Value |
Hardness, Rockwell F | 82 [-] Show Material materials with Hardness, Rockwell F of 82 [-] | Predicted Value |
Hardness, Rockwell Superficial 15-N | 74 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 74 [-] | Predicted Value |
Hardness, Rockwell Superficial 30-N | 47 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 47 [-] | Predicted Value |
Hardness, Rockwell Superficial 30-T | 89 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 89 [-] | Predicted Value |
Límite elástico | 563.7 MPa Show Material materials with Límite elástico of 563.7 MPa | Predicted Value, RP02 |
621.1 MPa Show Material materials with Límite elástico of 621.1 MPa | Predicted Value | |
708.3 MPa Show Material materials with Límite elástico of 708.3 MPa | Predicted Value, RP005 | |
Módulo de cizallamiento | 46.4 GPa Show Material materials with Módulo de cizallamiento of 46.4 GPa | Predicted Value |
Módulo elástico | 96 - 120 GPa Show Material materials with Módulo elástico of 96 - 120 GPa | Typical for Cast Copper Bronze |
Resistencia a la compresión | 1182 MPa Show Material materials with Resistencia a la compresión of 1182 MPa | Predicted Value |
Resistencia a la fatiga | 376 MPa Show Material materials with Resistencia a la fatiga of 376 MPa | Predicted Value |
Resistencia al cizallamiento | 420.7 MPa Show Material materials with Resistencia al cizallamiento of 420.7 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 376 - 440 J/(kg·K) Show Material materials with Calor específico of 376 - 440 J/(kg·K) | Typical for Cast Copper Bronze |
Coeficiente de dilatación térmica | 1.6e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6e-05 - 1.9e-05 1/K | Typical for Cast Copper Bronze |
Conductividad térmica | 12 - 81 W/(m·K) Show Material materials with Conductividad térmica of 12 - 81 W/(m·K) | Typical for Cast Copper Bronze |
Temperatura de fusión | 760 - 1060 °C Show Material materials with Temperatura de fusión of 760 - 1060 °C | Typical for Cast Copper Bronze |
Eléctrico
Chemical properties
Property | Value | Related Standards |
---|---|---|
Aluminio | 10.5 - 11.5 % Show Material materials with Aluminio of 10.5 - 11.5 % | ASTM B505 |
Cobre | 74.5 % Show Material materials with Cobre of 74.5 % | ASTM B505 |
Estaño | 0.25 % Show Material materials with Estaño of 0.25 % | ASTM B505 |
Hierro | 4 - 5.5 % Show Material materials with Hierro of 4 - 5.5 % | ASTM B505 |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % | ASTM B505 |
Níquel | 4.2 - 6 % Show Material materials with Níquel of 4.2 - 6 % | ASTM B505 |
Plomo | 0.03 % Show Material materials with Plomo of 0.03 % | ASTM B505 |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % | ASTM B505 |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % | ASTM B505 |