General
Property | Value | Comment |
---|---|---|
Densidad | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Tamaño de grano | 0.0303 μm Show Material materials with Tamaño de grano of 0.0303 μm | Predicted Value |
Mecánica
Property | Value | Related Standards | Shape | Comment |
---|---|---|---|---|
Coeficiente de Poisson | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass | ||
Dureza Brinell | 127 [-] Show Material materials with Dureza Brinell of 127 [-] | Predicted Value | ||
Dureza Brinell (HBW) | 244.4 [-] Show Material materials with Dureza Brinell (HBW) of 244.4 [-] | Predicted Value | ||
Dureza Vickers | 134 [-] Show Material materials with Dureza Vickers of 134 [-] | Predicted Value | ||
Estricción | 45.2 % Show Material materials with Estricción of 45.2 % | Predicted Value | ||
Hardness, Rockwell F | 75 [-] Show Material materials with Hardness, Rockwell F of 75 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 15-N | 71 [-] Show Material materials with Hardness, Rockwell Superficial 15-N of 71 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-N | 43 [-] Show Material materials with Hardness, Rockwell Superficial 30-N of 43 [-] | Predicted Value | ||
Hardness, Rockwell Superficial 30-T | 67 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 67 [-] | Predicted Value | ||
Módulo de cizallamiento | 43.4 GPa Show Material materials with Módulo de cizallamiento of 43.4 GPa | Predicted Value | ||
Módulo elástico | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass | ||
Resistencia a la compresión | 1162 MPa Show Material materials with Resistencia a la compresión of 1162 MPa | Predicted Value | ||
Resistencia a la fatiga | 377 MPa Show Material materials with Resistencia a la fatiga of 377 MPa | Predicted Value | ||
Resistencia a la tracción | 414 MPa Show Material materials with Resistencia a la tracción of 414 MPa | ASTM B584 | Casting | |
Resistencia al cizallamiento | 280.1 MPa Show Material materials with Resistencia al cizallamiento of 280.1 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 1.5e-05 - 1.9e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5e-05 - 1.9e-05 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Eléctrico
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Aluminio | 0.5 - 1.5 % Show Material materials with Aluminio of 0.5 - 1.5 % | ASTM B584 | Casting |
Cobre | 56 - 62 % Show Material materials with Cobre of 56 - 62 % | ASTM B584 | Casting |
Estaño | 0.5 - 1.5 % Show Material materials with Estaño of 0.5 - 1.5 % | ASTM B584 | Casting |
Hierro | 0.4 - 2 % Show Material materials with Hierro of 0.4 - 2 % | ASTM B584 | Casting |
Manganeso | 0.1 - 1 % Show Material materials with Manganeso of 0.1 - 1 % | ASTM B584 | Casting |
Níquel | 1 % Show Material materials with Níquel of 1 % | ASTM B584 | Casting |
Plomo | 0.5 - 1.5 % Show Material materials with Plomo of 0.5 - 1.5 % | ASTM B584 | Casting |
Zinc | 34 - 42 % Show Material materials with Zinc of 34 - 42 % | ASTM B584 | Casting |