General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Elongación A50 | 23.0 °C | 16 % Show Material materials with Elongación A50 of 16 % | |
Límite elástico Rp0.5 | 23.0 °C | 207 MPa Show Material materials with Límite elástico Rp0.5 of 207 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Resistencia a la tracción | 23.0 °C | 414 MPa Show Material materials with Resistencia a la tracción of 414 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 23.0 °C | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Cobre | 88 % Show Material materials with Cobre of 88 % |
Hierro | 0.2 % Show Material materials with Hierro of 0.2 % |
Manganeso | 0.25 % Show Material materials with Manganeso of 0.25 % |
Plomo | 0.09 % Show Material materials with Plomo of 0.09 % |
Silicona | 3.5 - 5.5 % Show Material materials with Silicona of 3.5 - 5.5 % |
Zinc | 4 - 7 % Show Material materials with Zinc of 4 - 7 % |