Mecánica
Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.15 % Show Material materials with Antimonio of 0.15 % |
Azufre | 0.05 % Show Material materials with Azufre of 0.05 % |
Cobre | 85 - 90 % Show Material materials with Cobre of 85 - 90 % |
Estaño | 4.5 - 6 % Show Material materials with Estaño of 4.5 - 6 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 4.5 - 6 % Show Material materials with Níquel of 4.5 - 6 % |
Plomo | 0.09 % Show Material materials with Plomo of 0.09 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Zinc | 1 - 2.5 % Show Material materials with Zinc of 1 - 2.5 % |