Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Elongación A50 | 23.0 °C | 3 % Show Material materials with Elongación A50 of 3 % | |
Límite elástico Rp 0,2 | 23.0 °C | 689 MPa Show Material materials with Límite elástico Rp 0,2 of 689 MPa | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Cast Copper Nickel Grade |
Resistencia a la tracción | 23.0 °C | 862 MPa Show Material materials with Resistencia a la tracción of 862 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.8E-5 1/K | Typical for Cast Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 23 - 45 W/(m·K) Show Material materials with Conductividad térmica of 23 - 45 W/(m·K) | Typical for Cast Copper Nickel Grade |
Temperatura de fusión | 1100 - 1240 °C Show Material materials with Temperatura de fusión of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Antimonio | 0.02 % Show Material materials with Antimonio of 0.02 % |
Azufre | 2.5E-3 % Show Material materials with Azufre of 2.5E-3 % |
Bismuto | 1E-3 % Show Material materials with Bismuto of 1E-3 % |
Estaño | 7.5 - 8.5 % Show Material materials with Estaño of 7.5 - 8.5 % |
Fósforo | 5E-3 % Show Material materials with Fósforo of 5E-3 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.05 - 0.3 % Show Material materials with Manganeso of 0.05 - 0.3 % |
Níquel | 9.5 - 10.5 % Show Material materials with Níquel of 9.5 - 10.5 % |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |