Mecánica
Chemical properties
Property | Value |
---|---|
Aluminio | 0.1 % Show Material materials with Aluminio of 0.1 % |
Antimonio | 0.02 % Show Material materials with Antimonio of 0.02 % |
Azufre | 2.5E-3 % Show Material materials with Azufre of 2.5E-3 % |
Bismuto | 1E-3 % Show Material materials with Bismuto of 1E-3 % |
Estaño | 7.5 - 8.5 % Show Material materials with Estaño of 7.5 - 8.5 % |
Fósforo | 5E-3 % Show Material materials with Fósforo of 5E-3 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Manganeso | 0.05 - 0.3 % Show Material materials with Manganeso of 0.05 - 0.3 % |
Níquel | 9.5 - 10.5 % Show Material materials with Níquel of 9.5 - 10.5 % |
Plomo | 5E-3 % Show Material materials with Plomo of 5E-3 % |
Silicona | 0.05 % Show Material materials with Silicona of 0.05 % |
Zinc | 1 % Show Material materials with Zinc of 1 % |