General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación A50 | 23.0 °C | 10 % Show Material materials with Elongación A50 of 10 % | |
Límite elástico Rp 0,2 | 23.0 °C | 90 - 110 MPa Show Material materials with Límite elástico Rp 0,2 of 90 - 110 MPa | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Resistencia a la tracción | 23.0 °C | 790 - 930 MPa Show Material materials with Resistencia a la tracción of 790 - 930 MPa | |
Yield strength Rp0.05 | 23.0 °C | 585 - 725 MPa Show Material materials with Yield strength Rp0.05 of 585 - 725 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Estaño | 4.5 - 5.5 % Show Material materials with Estaño of 4.5 - 5.5 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 7 - 8 % Show Material materials with Níquel of 7 - 8 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % |