General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.95 g/cm³ Show Material materials with Densidad of 8.95 g/cm³ | Typical for Wrought Copper Nickel Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación A50 | 23.0 °C | 6 % Show Material materials with Elongación A50 of 6 % | |
Límite elástico Rp 0,2 | 23.0 °C | 120 - 145 MPa Show Material materials with Límite elástico Rp 0,2 of 120 - 145 MPa | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Wrought Copper Nickel Grade |
Resistencia a la tracción | 23.0 °C | 895 - 1035 MPa Show Material materials with Resistencia a la tracción of 895 - 1035 MPa | |
Yield strength Rp0.05 | 23.0 °C | 725 - 895 MPa Show Material materials with Yield strength Rp0.05 of 725 - 895 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 375 - 398 J/(kg·K) Show Material materials with Calor específico of 375 - 398 J/(kg·K) | Typical for Wrought Copper Nickel Grade |
Coeficiente de dilatación térmica | 23.0 °C | 1.4E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 - 1.8E-5 1/K | Typical for Wrought Copper Nickel Grade |
Conductividad térmica | 23.0 °C | 21 - 195 W/(m·K) Show Material materials with Conductividad térmica of 21 - 195 W/(m·K) | Typical for Wrought Copper Nickel Grade |
Temperatura de fusión | 915 - 1240 °C Show Material materials with Temperatura de fusión of 915 - 1240 °C | Typical for Wrought Copper Nickel Grade |
Chemical properties
Property | Value |
---|---|
Estaño | 7.5 - 8.5 % Show Material materials with Estaño of 7.5 - 8.5 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Magnesio | 0.15 % Show Material materials with Magnesio of 0.15 % |
Manganeso | 0.3 % Show Material materials with Manganeso of 0.3 % |
Niobio | 0.1 % Show Material materials with Niobio of 0.1 % |
Níquel | 14.5 - 15.5 % Show Material materials with Níquel of 14.5 - 15.5 % |
Plomo | 0.02 % Show Material materials with Plomo of 0.02 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |