General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.47 g/cm³ Show Material materials with Densidad of 8.47 g/cm³ | Typical for Cast Copper Brass Yellow Brass |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Brass Yellow Brass |
Elongación A50 | 23.0 °C | 15 % Show Material materials with Elongación A50 of 15 % | |
Límite elástico Rp0.5 | 23.0 °C | 138 MPa Show Material materials with Límite elástico Rp0.5 of 138 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Cast Copper Brass Yellow Brass |
Resistencia a la tracción | 23.0 °C | 414 MPa Show Material materials with Resistencia a la tracción of 414 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 335 - 390 J/(kg·K) Show Material materials with Calor específico of 335 - 390 J/(kg·K) | Typical for Cast Copper Brass Yellow Brass |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Cast Copper Brass Yellow Brass |
Conductividad térmica | 23.0 °C | 116 W/(m·K) Show Material materials with Conductividad térmica of 116 W/(m·K) | Typical for Cast Copper Brass Yellow Brass |
Temperatura de fusión | 905 - 932 °C Show Material materials with Temperatura de fusión of 905 - 932 °C | Typical for Cast Copper Brass Yellow Brass |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 - 1.5 % Show Material materials with Aluminio of 0.5 - 1.5 % |
Cobre | 56 - 62 % Show Material materials with Cobre of 56 - 62 % |
Estaño | 0.5 - 1.5 % Show Material materials with Estaño of 0.5 - 1.5 % |
Hierro | 0.4 - 2 % Show Material materials with Hierro of 0.4 - 2 % |
Manganeso | 0.1 - 1.5 % Show Material materials with Manganeso of 0.1 - 1.5 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Plomo | 0.5 - 1.5 % Show Material materials with Plomo of 0.5 - 1.5 % |
Zinc | 34 - 42 % Show Material materials with Zinc of 34 - 42 % |