Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 190 [-] Show Material materials with Dureza Brinell of 190 [-] |
Elongación A50 | 20.0 °C | 6 % Show Material materials with Elongación A50 of 6 % |
Límite elástico Rp0.5 | 20.0 °C | 310 MPa Show Material materials with Límite elástico Rp0.5 of 310 MPa |
Resistencia a la tracción | 20.0 °C | 620 MPa Show Material materials with Resistencia a la tracción of 620 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 10 - 11.5 % Show Material materials with Aluminio of 10 - 11.5 % |
Cobre | 83 % Show Material materials with Cobre of 83 % |
Hierro | 3 - 5 % Show Material materials with Hierro of 3 - 5 % |
Manganeso | 0.5 % Show Material materials with Manganeso of 0.5 % |
Níquel | 1.5 % Show Material materials with Níquel of 1.5 % |