Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Rockwell B | 23.0 °C | 50 [-] Show Material materials with Dureza Rockwell B of 50 [-] | |
Límite elástico | 23.0 °C | 69 - 207 MPa Show Material materials with Límite elástico of 69 - 207 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Wrought Copper High Copper Alloy |
Resistencia a la tracción | 23.0 °C | 207 - 380 MPa Show Material materials with Resistencia a la tracción of 207 - 380 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 360 - 420 J/(kg·K) Show Material materials with Calor específico of 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper High Copper Alloy |
Temperatura de fusión | 855 - 1090 °C Show Material materials with Temperatura de fusión of 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.2 % Show Material materials with Aluminio of 0.2 % |
Berilio | 0.2 - 0.6 % Show Material materials with Berilio of 0.2 - 0.6 % |
Cobalto | 0.3 % Show Material materials with Cobalto of 0.3 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Níquel | 1.4 - 2.2 % Show Material materials with Níquel of 1.4 - 2.2 % |
Silicona | 0.2 % Show Material materials with Silicona of 0.2 % |