General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.7 g/cm³ Show Material materials with Densidad of 1.7 g/cm³ | Typical for Cast Rare Earth Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Elongación A50 | 23.0 °C | 2 % Show Material materials with Elongación A50 of 2 % | |
Límite elástico Rp 0,2 | 23.0 °C | 96 MPa Show Material materials with Límite elástico Rp 0,2 of 96 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Cast Rare Earth Grade |
Resistencia a la tracción | 23.0 °C | 138 MPa Show Material materials with Resistencia a la tracción of 138 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 966 - 1050 J/(kg·K) Show Material materials with Calor específico of 966 - 1050 J/(kg·K) | Typical for Cast Rare Earth Grade |
Coeficiente de dilatación térmica | 23.0 °C | 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.6E-5 1/K | Typical for Cast Rare Earth Grade |
Conductividad térmica | 23.0 °C | 51 - 113 W/(m·K) Show Material materials with Conductividad térmica of 51 - 113 W/(m·K) | Typical for Cast Rare Earth Grade |
Temperatura de fusión | 535 - 645 °C Show Material materials with Temperatura de fusión of 535 - 645 °C | Typical for Cast Rare Earth Grade |
Chemical properties
Property | Value |
---|---|
Circonio | 0.5 - 1 % Show Material materials with Circonio of 0.5 - 1 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Níquel | 0.01 % Show Material materials with Níquel of 0.01 % |
Tierras raras | 2.5 - 4 % Show Material materials with Tierras raras of 2.5 - 4 % |
Zinc | 2 - 3.1 % Show Material materials with Zinc of 2 - 3.1 % |