General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.7 g/cm³ Show Material materials with Densidad of 1.7 g/cm³ | Typical for Cast Rare Earth Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Elongación A50 | 23.0 °C | 2 % Show Material materials with Elongación A50 of 2 % | |
Límite elástico Rp 0,2 | 23.0 °C | 179 MPa Show Material materials with Límite elástico Rp 0,2 of 179 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Cast Rare Earth Grade |
Resistencia a la tracción | 23.0 °C | 255 MPa Show Material materials with Resistencia a la tracción of 255 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 966 - 1050 J/(kg·K) Show Material materials with Calor específico of 966 - 1050 J/(kg·K) | Typical for Cast Rare Earth Grade |
Coeficiente de dilatación térmica | 23.0 °C | 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.6E-5 1/K | Typical for Cast Rare Earth Grade |
Conductividad térmica | 23.0 °C | 51 - 113 W/(m·K) Show Material materials with Conductividad térmica of 51 - 113 W/(m·K) | Typical for Cast Rare Earth Grade |
Temperatura de fusión | 535 - 645 °C Show Material materials with Temperatura de fusión of 535 - 645 °C | Typical for Cast Rare Earth Grade |
Chemical properties
Property | Value |
---|---|
Circonio | 0.4 - 1 % Show Material materials with Circonio of 0.4 - 1 % |
Cobre | 0.03 % Show Material materials with Cobre of 0.03 % |
Itrio | 4.75 - 5.5 % Show Material materials with Itrio of 4.75 - 5.5 % |
Litio | 0.2 % Show Material materials with Litio of 0.2 % |
Manganeso | 0.03 % Show Material materials with Manganeso of 0.03 % |
Neodimio | 2 % Show Material materials with Neodimio of 2 % |
Níquel | 5E-3 % Show Material materials with Níquel of 5E-3 % |
Silicona | 0.01 % Show Material materials with Silicona of 0.01 % |
Tierras raras | 2 % Show Material materials with Tierras raras of 2 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |