General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | Typical for Cast Aluminium Manganese Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Dureza Brinell | 23.0 °C | 62 [-] Show Material materials with Dureza Brinell of 62 [-] | |
Elongación A50 | 23.0 °C | 8 % Show Material materials with Elongación A50 of 8 % | |
Límite elástico | 23.0 °C | 130 MPa Show Material materials with Límite elástico of 130 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Cast Aluminium Manganese Grade |
Resistencia a la tracción | 23.0 °C | 220 MPa Show Material materials with Resistencia a la tracción of 220 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 1000 - 1080 J/(kg·K) Show Material materials with Calor específico of 1000 - 1080 J/(kg·K) | Typical for Cast Aluminium Manganese Grade |
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 - 2.6E-5 1/K | Typical for Cast Aluminium Manganese Grade |
Conductividad térmica | 23.0 °C | 42 - 75 W/(m·K) Show Material materials with Conductividad térmica of 42 - 75 W/(m·K) | Typical for Cast Aluminium Manganese Grade |
Temperatura de fusión | 465 - 620 °C Show Material materials with Temperatura de fusión of 465 - 620 °C | Typical for Cast Aluminium Manganese Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 5.5 - 6.5 % Show Material materials with Aluminio of 5.5 - 6.5 % |
Cobre | 0.01 % Show Material materials with Cobre of 0.01 % |
Hierro | 5E-3 % Show Material materials with Hierro of 5E-3 % |
Manganeso | 0.24 - 0.6 % Show Material materials with Manganeso of 0.24 - 0.6 % |
Níquel | 2E-3 % Show Material materials with Níquel of 2E-3 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |
Zinc | 0.22 % Show Material materials with Zinc of 0.22 % |