General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 2.72 g/cm³ Show Material materials with Densidad of 2.72 g/cm³ | Typical for Cast Aluminium Manganese Grade |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Límite elástico Rp 0,2 | 23.0 °C | 117 MPa Show Material materials with Límite elástico Rp 0,2 of 117 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 40 - 45 GPa Show Material materials with Módulo elástico of 40 - 45 GPa | Typical for Cast Aluminium Manganese Grade |
Resistencia a la tracción | 23.0 °C | 234 MPa Show Material materials with Resistencia a la tracción of 234 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 1000 - 1080 J/(kg·K) Show Material materials with Calor específico of 1000 - 1080 J/(kg·K) | Typical for Cast Aluminium Manganese Grade |
Coeficiente de dilatación térmica | 23.0 °C | 2.5E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.5E-5 - 2.6E-5 1/K | Typical for Cast Aluminium Manganese Grade |
Conductividad térmica | 23.0 °C | 42 - 75 W/(m·K) Show Material materials with Conductividad térmica of 42 - 75 W/(m·K) | Typical for Cast Aluminium Manganese Grade |
Temperatura de fusión | 465 - 620 °C Show Material materials with Temperatura de fusión of 465 - 620 °C | Typical for Cast Aluminium Manganese Grade |
Chemical properties
Property | Value |
---|---|
Aluminio | 9.3 - 10.7 % Show Material materials with Aluminio of 9.3 - 10.7 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Manganeso | 0.1 - 0.35 % Show Material materials with Manganeso of 0.1 - 0.35 % |
Níquel | 0.01 % Show Material materials with Níquel of 0.01 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |