General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.74 g/cm³ Show Material materials with Densidad of 1.74 g/cm³ | Typical for Magnesium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Elongación | 23.0 °C | 2.5 % Show Material materials with Elongación of 2.5 % | |
Límite elástico Rp 0,2 | 23.0 °C | 133 MPa Show Material materials with Límite elástico Rp 0,2 of 133 MPa | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 23.0 °C | 45 GPa Show Material materials with Módulo elástico of 45 GPa | Typical for Magnesium |
Resistencia a la tracción | 23.0 °C | 200 MPa Show Material materials with Resistencia a la tracción of 200 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Calor específico of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Conductividad térmica | 23.0 °C | 153 - 167 W/(m·K) Show Material materials with Conductividad térmica of 153 - 167 W/(m·K) | Typical for Magnesium |
Temperatura de fusión | 650 °C Show Material materials with Temperatura de fusión of 650 °C | Typical for Magnesium |
Chemical properties
Property | Value |
---|---|
Circonio | 0.4 - 1 % Show Material materials with Circonio of 0.4 - 1 % |
Cobre | 0.1 % Show Material materials with Cobre of 0.1 % |
Manganeso | 0.15 % Show Material materials with Manganeso of 0.15 % |
Níquel | 0.01 % Show Material materials with Níquel of 0.01 % |
Tierras raras | 0.75 - 1.75 % Show Material materials with Tierras raras of 0.75 - 1.75 % |
Zinc | 3.5 - 5 % Show Material materials with Zinc of 3.5 - 5 % |