General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 2.65 - 2.7 g/cm³ Show Material materials with Densidad of 2.65 - 2.7 g/cm³ | Typical for Wrought 5000 Series Aluminium |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Wrought 5000 Series Aluminium |
Módulo de cizallamiento | 20.0 °C | 26 - 26.5 GPa Show Material materials with Módulo de cizallamiento of 26 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium |
Módulo elástico | 20.0 °C | 69 - 70 GPa Show Material materials with Módulo elástico of 69 - 70 GPa | Typical for Wrought 5000 Series Aluminium |
Resistencia a la fractura | 20.0 °C | 22 - 35 MPa·√m Show Material materials with Resistencia a la fractura of 22 - 35 MPa·√m | Typical for Wrought 5000 Series Aluminium |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 879 - 963 J/(kg·K) Show Material materials with Calor específico of 879 - 963 J/(kg·K) | Typical for Wrought 5000 Series Aluminium |
Coeficiente de dilatación térmica | 20.0 °C | 2.2E-5 - 2.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.2E-5 - 2.5E-5 1/K | Typical for Wrought 5000 Series Aluminium |
Conductividad térmica | 20.0 °C | 112 - 205 W/(m·K) Show Material materials with Conductividad térmica of 112 - 205 W/(m·K) | Typical for Wrought 5000 Series Aluminium |
Temperatura de fusión | 600 - 650 °C Show Material materials with Temperatura de fusión of 600 - 650 °C | Typical for Wrought 5000 Series Aluminium | |
Temperatura máx. de funcionamiento | 150 °C Show Material materials with Temperatura máx. de funcionamiento of 150 °C | Typical for Wrought 5000 Series Aluminium |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Conductividad eléctrica | 20.0 °C | 1.80E+7 - 3.10E+7 S/m Show Material materials with Conductividad eléctrica of 1.80E+7 - 3.10E+7 S/m | Typical for Wrought 5000 Series Aluminium |
Resistividad eléctrica | 20.0 °C | 3.3E-8 - 5E-8 Ω·m Show Material materials with Resistividad eléctrica of 3.3E-8 - 5E-8 Ω·m | Typical for Wrought 5000 Series Aluminium |
Chemical properties
Property | Value |
---|---|
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Cromo | 0.1 % Show Material materials with Cromo of 0.1 % |
Hierro | 0.7 % Show Material materials with Hierro of 0.7 % |
Magnesio | 0.5 - 1.1 % Show Material materials with Magnesio of 0.5 - 1.1 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Zinc | 0.25 % Show Material materials with Zinc of 0.25 % |
Technological properties
Property | ||
---|---|---|
Workability | Good workability. |