General
Property | Value | Comment |
---|---|---|
Densidad | 2.6 - 2.7 g/cm³ Show Material materials with Densidad of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mecánica
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coeficiente de Poisson | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Dureza Brinell | 75.0 [-] Show Material materials with Dureza Brinell of 75.0 [-] | T4 | ASTM B618 | Casting | |
Elongación | 10.0 % Show Material materials with Elongación of 10.0 % | T4 | ASTM B618 | Casting | |
Módulo elástico | 68.0 - 70.0 GPa Show Material materials with Módulo elástico of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | |||
Resistencia a la tracción | 290.0 MPa Show Material materials with Resistencia a la tracción of 290.0 MPa | T4 | ASTM B618 | Casting |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 963.0 J/(kg·K) Show Material materials with Calor específico of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium |
Coeficiente de dilatación térmica | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium |
Conductividad térmica | 60.0 - 140.0 W/(m·K) Show Material materials with Conductividad térmica of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Temperatura de fusión | 450.0 - 640.0 °C Show Material materials with Temperatura de fusión of 450.0 - 640.0 °C | Typical for Cast 5xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Cobre | 0.25 Show Material materials with Cobre of 0.25 | T4 | ASTM B618 | Casting |
Hierro | 0.3 Show Material materials with Hierro of 0.3 | T4 | ASTM B618 | Casting |
Magnesio | 9.5 - 10.6 % Show Material materials with Magnesio of 9.5 - 10.6 % | T4 | ASTM B618 | Casting |
Manganeso | 0.15 Show Material materials with Manganeso of 0.15 | T4 | ASTM B618 | Casting |
Silicona | 0.25 Show Material materials with Silicona of 0.25 | T4 | ASTM B618 | Casting |
Titanio | 0.25 Show Material materials with Titanio of 0.25 | T4 | ASTM B618 | Casting |
Zinc | 0.15 Show Material materials with Zinc of 0.15 | T4 | ASTM B618 | Casting |