Mecánica
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.6 - 0.75 % Show Material materials with Carbono of 0.6 - 0.75 % |
Cromo | 16 - 18 % Show Material materials with Cromo of 16 - 18 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Hierro | 77.83 - 83.4 % Show Material materials with Hierro of 77.83 - 83.4 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 0.75 % Show Material materials with Molibdeno of 0.75 % |
Níquel | 0.6 % Show Material materials with Níquel of 0.6 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Technological properties
Property | ||
---|---|---|
Processing history | cold-rolled, annealed, quenched and tempered |