General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 6.8 - 7.8 g/cm³ Show Material materials with Densidad of 6.8 - 7.8 g/cm³ | Typical for Cast Iron |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell (HBW) | 23.0 °C | 241 - 302 [-] Show Material materials with Dureza Brinell (HBW) of 241 - 302 [-] | |
Elongación | 23.0 °C | 3 % Show Material materials with Elongación of 3 % | |
Límite elástico | 23.0 °C | 425 - 450 MPa Show Material materials with Límite elástico of 425 - 450 MPa | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 23.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa | |
Resistencia a la tracción | 23.0 °C | 700 MPa Show Material materials with Resistencia a la tracción of 700 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 - 527 J/(kg·K) Show Material materials with Calor específico of 460 - 527 J/(kg·K) | Typical for Cast Iron |
Conductividad térmica | 23.0 °C | 55 W/(m·K) Show Material materials with Conductividad térmica of 55 W/(m·K) | Typical for Cast Iron |
Temperatura de fusión | 1120 °C Show Material materials with Temperatura de fusión of 1120 °C | Typical for Cast Iron |
Chemical properties
Property | Value |
---|---|
Azufre | 0.005 - 0.035 % Show Material materials with Azufre of 0.005 - 0.035 % |
Carbono | 3.2 - 4.1 % Show Material materials with Carbono of 3.2 - 4.1 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | balance |
Manganeso | 0.1 - 1 % Show Material materials with Manganeso of 0.1 - 1 % |
Silicona | 1.8 - 3 % Show Material materials with Silicona of 1.8 - 3 % |