General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación transversal | 20.0 °C | 19 % Show Material materials with Elongación transversal of 19 % | |
Límite elástico | 20.0 °C | 385 MPa Show Material materials with Límite elástico of 385 MPa | |
Límite elástico transversal | 20.0 °C | 385 MPa Show Material materials with Límite elástico transversal of 385 MPa | |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 530 - 680 MPa Show Material materials with Resistencia a la tracción of 530 - 680 MPa | |
Resistencia a la tracción transversal | 20.0 °C | 530 - 680 MPa Show Material materials with Resistencia a la tracción transversal of 530 - 680 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.02 % Show Material materials with Aluminio of 0.02 % |
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.23 % Show Material materials with Carbono of 0.23 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1 - 1.5 % Show Material materials with Manganeso of 1 - 1.5 % |
Silicona | 0.55 % Show Material materials with Silicona of 0.55 % |